Kinetic aspects on ferric arsenate formation in a fix bed gas-solid reaction system
The fixation of arsenic contained in gases produced during pyrometallurgical processes by using solid ferric oxide was studied in the range 873-1073 K under different oxygen potential and solid aggregates porosities. Arsenic fixation on solid iron oxides is described by the pore blocking model under...
- Autores:
-
Balladares, Eduardo
Parra, Roberto
Sánchez, Mario
- Tipo de recurso:
- Article of journal
- Fecha de publicación:
- 2015
- Institución:
- Universidad Nacional de Colombia
- Repositorio:
- Universidad Nacional de Colombia
- Idioma:
- spa
- OAI Identifier:
- oai:repositorio.unal.edu.co:unal/60768
- Acceso en línea:
- https://repositorio.unal.edu.co/handle/unal/60768
http://bdigital.unal.edu.co/59100/
- Palabra clave:
- 62 Ingeniería y operaciones afines / Engineering
arsenic fixation
flue dust
gas treatment
copper smelting.
- Rights
- openAccess
- License
- Atribución-NoComercial 4.0 Internacional