Impact of Glass Fiber Content and Packing Pressure on Weld Line Integrity in Injection Molded Short Glass Fibre Reinforced Polyamide

Managing the challenge of weld lines of short-fiber reinforced polymers (SFRPs) in injection molding is crucial for enhancing the mechanical performance of these composites. This study evaluates the impact of various glass fiber contents (0 to 50 wt%) within a polyamide 6 (PA6) matrix on the tensile...

Full description

Autores:
Mokarizadehhaghighishirazi, Majid
Buffel, Bart
Lomov, Stepan V.
Desplentere, Frederik
Tipo de recurso:
Conferencia (Ponencia)
Fecha de publicación:
2024
Institución:
Universidad de los Andes
Repositorio:
Séneca: repositorio Uniandes
Idioma:
eng
OAI Identifier:
oai:repositorio.uniandes.edu.co:1992/76074
Acceso en línea:
https://hdl.handle.net/1992/76074
https://doi.org/10.51573/Andes.PPS39.GS.IM.2
https://repositorio.uniandes.edu.co/
Palabra clave:
Injection Molding
Short-Fiber Reinforced Polymer
Weld Lines
Fiber Orientation
Ingeniería
Rights
openAccess
License
https://repositorio.uniandes.edu.co/static/pdf/aceptacion_uso_es.pdf
id UNIANDES2_13c8f5880455bdedd943bb6c4ccbeea2
oai_identifier_str oai:repositorio.uniandes.edu.co:1992/76074
network_acronym_str UNIANDES2
network_name_str Séneca: repositorio Uniandes
repository_id_str
dc.title.none.fl_str_mv Impact of Glass Fiber Content and Packing Pressure on Weld Line Integrity in Injection Molded Short Glass Fibre Reinforced Polyamide
title Impact of Glass Fiber Content and Packing Pressure on Weld Line Integrity in Injection Molded Short Glass Fibre Reinforced Polyamide
spellingShingle Impact of Glass Fiber Content and Packing Pressure on Weld Line Integrity in Injection Molded Short Glass Fibre Reinforced Polyamide
Injection Molding
Short-Fiber Reinforced Polymer
Weld Lines
Fiber Orientation
Ingeniería
title_short Impact of Glass Fiber Content and Packing Pressure on Weld Line Integrity in Injection Molded Short Glass Fibre Reinforced Polyamide
title_full Impact of Glass Fiber Content and Packing Pressure on Weld Line Integrity in Injection Molded Short Glass Fibre Reinforced Polyamide
title_fullStr Impact of Glass Fiber Content and Packing Pressure on Weld Line Integrity in Injection Molded Short Glass Fibre Reinforced Polyamide
title_full_unstemmed Impact of Glass Fiber Content and Packing Pressure on Weld Line Integrity in Injection Molded Short Glass Fibre Reinforced Polyamide
title_sort Impact of Glass Fiber Content and Packing Pressure on Weld Line Integrity in Injection Molded Short Glass Fibre Reinforced Polyamide
dc.creator.fl_str_mv Mokarizadehhaghighishirazi, Majid
Buffel, Bart
Lomov, Stepan V.
Desplentere, Frederik
dc.contributor.author.none.fl_str_mv Mokarizadehhaghighishirazi, Majid
Buffel, Bart
Lomov, Stepan V.
Desplentere, Frederik
dc.contributor.editor.none.fl_str_mv Salcedo, Felipe
Perilla, Jairo Ernesto
Sierra, Cesar
Medina, Jorge Alberto
dc.subject.keyword.none.fl_str_mv Injection Molding
Short-Fiber Reinforced Polymer
Weld Lines
Fiber Orientation
topic Injection Molding
Short-Fiber Reinforced Polymer
Weld Lines
Fiber Orientation
Ingeniería
dc.subject.themes.none.fl_str_mv Ingeniería
description Managing the challenge of weld lines of short-fiber reinforced polymers (SFRPs) in injection molding is crucial for enhancing the mechanical performance of these composites. This study evaluates the impact of various glass fiber contents (0 to 50 wt%) within a polyamide 6 (PA6) matrix on the tensile and flexural properties at weld lines, comparing each sample to its counterpart without a weld line. Our findings indicate that weld lines have minimal impact on the mechanical properties of composites with low fiber content (10 wt%). However, at higher fiber contents, the strength, modulus, and strain at fracture are significantly reduced due to unfavorable fiber orientations at the weld lines. Increasing the packing pressure during injection molding can partially recover these properties by promoting favorable fiber orientation at the weld line. This signifies the importance of carefully controlling processing parameters to optimize the mechanical performance of SFRPs at weld lines.
publishDate 2024
dc.date.issued.none.fl_str_mv 2024-12
dc.date.accessioned.none.fl_str_mv 2025-02-07T21:40:36Z
dc.date.available.none.fl_str_mv 2025-02-07T21:40:36Z
dc.type.none.fl_str_mv Documento de Conferencia
dc.type.coar.fl_str_mv http://purl.org/coar/resource_type/c_c94f
dc.type.driver.none.fl_str_mv info:eu-repo/semantics/conferenceObject
dc.type.version.none.fl_str_mv info:eu-repo/semantics/publishedVersion
dc.type.coar.none.fl_str_mv http://purl.org/coar/resource_type/c_8544
dc.type.coarversion.none.fl_str_mv http://purl.org/coar/version/c_970fb48d4fbd8a85
dc.type.content.none.fl_str_mv Text
format http://purl.org/coar/resource_type/c_8544
status_str publishedVersion
dc.identifier.isbn.none.fl_str_mv 978-958-798-779-9
dc.identifier.uri.none.fl_str_mv https://hdl.handle.net/1992/76074
dc.identifier.doi.none.fl_str_mv https://doi.org/10.51573/Andes.PPS39.GS.IM.2
dc.identifier.instname.none.fl_str_mv Universidad de los Andes
dc.identifier.reponame.none.fl_str_mv Repositorio Institucional Séneca
dc.identifier.repourl.none.fl_str_mv https://repositorio.uniandes.edu.co/
identifier_str_mv 978-958-798-779-9
Universidad de los Andes
Repositorio Institucional Séneca
url https://hdl.handle.net/1992/76074
https://doi.org/10.51573/Andes.PPS39.GS.IM.2
https://repositorio.uniandes.edu.co/
dc.language.iso.none.fl_str_mv eng
language eng
dc.relation.conferencedate.none.fl_str_mv 05-19-2024/05-23-2024
dc.relation.conferenceplace.none.fl_str_mv Cartagena de Indias, Colombia
dc.relation.ispartofconference.none.fl_str_mv Proceedings of the 39th International Conference of the Polymer Processing Society (PPS-39)
dc.rights.uri.none.fl_str_mv https://repositorio.uniandes.edu.co/static/pdf/aceptacion_uso_es.pdf
dc.rights.accessrights.none.fl_str_mv info:eu-repo/semantics/openAccess
dc.rights.coar.none.fl_str_mv http://purl.org/coar/access_right/c_abf2
rights_invalid_str_mv https://repositorio.uniandes.edu.co/static/pdf/aceptacion_uso_es.pdf
http://purl.org/coar/access_right/c_abf2
eu_rights_str_mv openAccess
dc.format.extent.none.fl_str_mv 10 páginas
dc.format.mimetype.none.fl_str_mv application/pdf
dc.publisher.none.fl_str_mv Ediciones Uniandes
dc.publisher.faculty.none.fl_str_mv Facultad de Ingeniería
dc.publisher.place.none.fl_str_mv Bogotá
publisher.none.fl_str_mv Ediciones Uniandes
institution Universidad de los Andes
bitstream.url.fl_str_mv https://repositorio.uniandes.edu.co/bitstreams/98183eda-1319-496e-babc-e8f7426ba16e/download
https://repositorio.uniandes.edu.co/bitstreams/e9fa88f4-5706-4899-8864-de8c2c387afc/download
https://repositorio.uniandes.edu.co/bitstreams/37d829e7-4c07-4e71-9c16-91a6a1f6d93c/download
https://repositorio.uniandes.edu.co/bitstreams/1d88f547-231c-4f67-95c9-3162d000f636/download
https://repositorio.uniandes.edu.co/bitstreams/e133483a-3532-4df5-b895-2e1a8045d8eb/download
https://repositorio.uniandes.edu.co/bitstreams/d32bef4d-a3cb-4a05-b067-a8752750012c/download
https://repositorio.uniandes.edu.co/bitstreams/3870d1ca-e149-4485-bc15-c3480ab2a596/download
bitstream.checksum.fl_str_mv 016b58bf0ac806b1f5cc2d738616c233
a50091f3c8d9cd8581b2acf519df6624
ae9e573a68e7f92501b6913cc846c39f
063f9ba8e5a2cbc8275f7e14640fa70a
696bc6269a5e4b4e49c95b23871f39e6
0ca370a6a0653a72ff13d14d8c4fa426
f211933ecdb059f1d7a6b07db3c1da79
bitstream.checksumAlgorithm.fl_str_mv MD5
MD5
MD5
MD5
MD5
MD5
MD5
repository.name.fl_str_mv Repositorio institucional Séneca
repository.mail.fl_str_mv adminrepositorio@uniandes.edu.co
_version_ 1831927670919659520
spelling Mokarizadehhaghighishirazi, MajidBuffel, BartLomov, Stepan V.Desplentere, FrederikSalcedo, FelipePerilla, Jairo ErnestoSierra, CesarMedina, Jorge Alberto2025-02-07T21:40:36Z2025-02-07T21:40:36Z2024-12978-958-798-779-9https://hdl.handle.net/1992/76074https://doi.org/10.51573/Andes.PPS39.GS.IM.2Universidad de los AndesRepositorio Institucional Sénecahttps://repositorio.uniandes.edu.co/Managing the challenge of weld lines of short-fiber reinforced polymers (SFRPs) in injection molding is crucial for enhancing the mechanical performance of these composites. This study evaluates the impact of various glass fiber contents (0 to 50 wt%) within a polyamide 6 (PA6) matrix on the tensile and flexural properties at weld lines, comparing each sample to its counterpart without a weld line. Our findings indicate that weld lines have minimal impact on the mechanical properties of composites with low fiber content (10 wt%). However, at higher fiber contents, the strength, modulus, and strain at fracture are significantly reduced due to unfavorable fiber orientations at the weld lines. Increasing the packing pressure during injection molding can partially recover these properties by promoting favorable fiber orientation at the weld line. This signifies the importance of carefully controlling processing parameters to optimize the mechanical performance of SFRPs at weld lines.10 páginasapplication/pdfengEdiciones UniandesFacultad de IngenieríaBogotáhttps://repositorio.uniandes.edu.co/static/pdf/aceptacion_uso_es.pdfinfo:eu-repo/semantics/openAccesshttp://purl.org/coar/access_right/c_abf2Impact of Glass Fiber Content and Packing Pressure on Weld Line Integrity in Injection Molded Short Glass Fibre Reinforced PolyamideDocumento de Conferenciainfo:eu-repo/semantics/conferenceObjectinfo:eu-repo/semantics/publishedVersionhttp://purl.org/coar/resource_type/c_8544http://purl.org/coar/resource_type/c_c94fhttp://purl.org/coar/version/c_970fb48d4fbd8a85TextInjection MoldingShort-Fiber Reinforced PolymerWeld LinesFiber OrientationIngeniería05-19-2024/05-23-2024Cartagena de Indias, ColombiaProceedings of the 39th International Conference of the Polymer Processing Society (PPS-39)ORIGINALPPS-39 - Impact of Glass Fiber Content and Packing Pressure on Weld Line Integrity in Injection Molded Short Glass Fibre Reinforced Polyamide.pdfPPS-39 - Impact of Glass Fiber Content and Packing Pressure on Weld Line Integrity in Injection Molded Short Glass Fibre Reinforced Polyamide.pdfapplication/pdf883513https://repositorio.uniandes.edu.co/bitstreams/98183eda-1319-496e-babc-e8f7426ba16e/download016b58bf0ac806b1f5cc2d738616c233MD51S04-87_LICENCIA Impact of Glass Fiber Content and Packing Pressure.pdfHIDEapplication/pdf296501https://repositorio.uniandes.edu.co/bitstreams/e9fa88f4-5706-4899-8864-de8c2c387afc/downloada50091f3c8d9cd8581b2acf519df6624MD55LICENSElicense.txtlicense.txttext/plain; charset=utf-82535https://repositorio.uniandes.edu.co/bitstreams/37d829e7-4c07-4e71-9c16-91a6a1f6d93c/downloadae9e573a68e7f92501b6913cc846c39fMD52TEXTPPS-39 - Impact of Glass Fiber Content and Packing Pressure on Weld Line Integrity in Injection Molded Short Glass Fibre Reinforced Polyamide.pdf.txtPPS-39 - Impact of Glass Fiber Content and Packing Pressure on Weld Line Integrity in Injection Molded Short Glass Fibre Reinforced Polyamide.pdf.txtExtracted texttext/plain18201https://repositorio.uniandes.edu.co/bitstreams/1d88f547-231c-4f67-95c9-3162d000f636/download063f9ba8e5a2cbc8275f7e14640fa70aMD53S04-87_LICENCIA Impact of Glass Fiber Content and Packing Pressure.pdf.txtS04-87_LICENCIA Impact of Glass Fiber Content and Packing Pressure.pdf.txtExtracted texttext/plain2163https://repositorio.uniandes.edu.co/bitstreams/e133483a-3532-4df5-b895-2e1a8045d8eb/download696bc6269a5e4b4e49c95b23871f39e6MD56THUMBNAILPPS-39 - Impact of Glass Fiber Content and Packing Pressure on Weld Line Integrity in Injection Molded Short Glass Fibre Reinforced Polyamide.pdf.jpgPPS-39 - Impact of Glass Fiber Content and Packing Pressure on Weld Line Integrity in Injection Molded Short Glass Fibre Reinforced Polyamide.pdf.jpgGenerated Thumbnailimage/jpeg8105https://repositorio.uniandes.edu.co/bitstreams/d32bef4d-a3cb-4a05-b067-a8752750012c/download0ca370a6a0653a72ff13d14d8c4fa426MD54S04-87_LICENCIA Impact of Glass Fiber Content and Packing Pressure.pdf.jpgS04-87_LICENCIA Impact of Glass Fiber Content and Packing Pressure.pdf.jpgGenerated Thumbnailimage/jpeg10831https://repositorio.uniandes.edu.co/bitstreams/3870d1ca-e149-4485-bc15-c3480ab2a596/downloadf211933ecdb059f1d7a6b07db3c1da79MD571992/76074oai:repositorio.uniandes.edu.co:1992/760742025-03-05 10:12:00.81https://repositorio.uniandes.edu.co/static/pdf/aceptacion_uso_es.pdfopen.accesshttps://repositorio.uniandes.edu.coRepositorio institucional Sénecaadminrepositorio@uniandes.edu.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