Structural characterization on batio3/la2/3ca1/3mno3 bilayers deposited on nb:srtio3
In this work we have investigated structural properties of La2/3Ca1/3MnO3/BaTiO3 bilayers grown on Nb:SrTiO3 substrates. The films were deposited by pulsed laser deposition (PLD) technique at high-pressure oxygen atmosphere and at a substrate temperature of 820 °C. . We report here the effect of the...
- Autores:
-
Ordoñez, John E.
Prieto, Pedro
Goméz, María E.
Lopera, Wilson
- Tipo de recurso:
- Article of journal
- Fecha de publicación:
- 2014
- Institución:
- Universidad Nacional de Colombia
- Repositorio:
- Universidad Nacional de Colombia
- Idioma:
- spa
- OAI Identifier:
- oai:repositorio.unal.edu.co:unal/50922
- Acceso en línea:
- https://repositorio.unal.edu.co/handle/unal/50922
http://bdigital.unal.edu.co/44964/
- Palabra clave:
- multifunctional materials
multiferroic oxides
ferroelectricity
ferromagnetism
materiales multifuncionales
multiferroicos
óxidos
ferroelectricidad
ferromagnetismo
- Rights
- openAccess
- License
- Atribución-NoComercial 4.0 Internacional
Summary: | In this work we have investigated structural properties of La2/3Ca1/3MnO3/BaTiO3 bilayers grown on Nb:SrTiO3 substrates. The films were deposited by pulsed laser deposition (PLD) technique at high-pressure oxygen atmosphere and at a substrate temperature of 820 °C. . We report here the effect of the thickness of the ferroelectric BaTiO3 layer on the structural properties of the ferromagnetic La2/3Ca1/3MnO3. We choose nominal thickness for the ferroelectric layer of 20, 50 and 100nm maintaining constant the ferromagnetic layer at 50 nm. The structural study in the bilayers by X-ray diffraction shows us that the Bragg angle of the La2/3Ca1/3MnO3 layer maintains the same position that that for a 50 nm-thick La2/3Ca1/3MnO3 layer, whereas the position of the BaTiO3 peak shifts toward lower angles indicating that the BTO layer grew with more internal stress than that for the individual 50 nm-thick BaTiO3 film gown under identical parameters (oxygen pressure and substrate temperature 400 mTorr for La2/3Ca1/3MnO3 (LCMO) and 3.0 mTorr for BaTiO3 (BTO)). |
---|