Propiedades mecánicas, eléctricas y de durabilidad de concretos con agregados reciclados
The purpose of this article is to present the assessment of some of the electrical, mechanical and durability properties of concrete mixtures with replacement of coarse aggregate by aggregates of recycled concrete (ACR). The ACR used in the mixtures of the tests was produced from the crushing of con...
- Autores:
-
Valverde Valverde, Jorge Alejandro
Torres Castellanos, Nancy
- Tipo de recurso:
- Article of journal
- Fecha de publicación:
- 2017
- Institución:
- Escuela Colombiana de Ingeniería Julio Garavito
- Repositorio:
- Repositorio Institucional ECI
- Idioma:
- spa
- OAI Identifier:
- oai:repositorio.escuelaing.edu.co:001/885
- Acceso en línea:
- http://revistas.escuelaing.edu.co/index.php/reci/article/view/15/11
https://repositorio.escuelaing.edu.co/handle/001/885
- Palabra clave:
- Agregados reciclados
Resistencia a la comprensión
Propiedades mecánicas
Durabilidad
Comprensión - Pruebas
Materiales - Propiedades mecánicas
Comprehension - Testing
Material - Mechanical properties
Recycled aggregates
Resistance to understanding
Mechanical properties
Durability
- Rights
- openAccess
- License
- Derechos Reservados - Escuela Colombiana de Ingeniería Julio Garavito
id |
ESCUELAIG2_4a5af156426fef678284670a089ee6fa |
---|---|
oai_identifier_str |
oai:repositorio.escuelaing.edu.co:001/885 |
network_acronym_str |
ESCUELAIG2 |
network_name_str |
Repositorio Institucional ECI |
repository_id_str |
|
dc.title.spa.fl_str_mv |
Propiedades mecánicas, eléctricas y de durabilidad de concretos con agregados reciclados |
title |
Propiedades mecánicas, eléctricas y de durabilidad de concretos con agregados reciclados |
spellingShingle |
Propiedades mecánicas, eléctricas y de durabilidad de concretos con agregados reciclados Agregados reciclados Resistencia a la comprensión Propiedades mecánicas Durabilidad Comprensión - Pruebas Materiales - Propiedades mecánicas Comprehension - Testing Material - Mechanical properties Recycled aggregates Resistance to understanding Mechanical properties Durability |
title_short |
Propiedades mecánicas, eléctricas y de durabilidad de concretos con agregados reciclados |
title_full |
Propiedades mecánicas, eléctricas y de durabilidad de concretos con agregados reciclados |
title_fullStr |
Propiedades mecánicas, eléctricas y de durabilidad de concretos con agregados reciclados |
title_full_unstemmed |
Propiedades mecánicas, eléctricas y de durabilidad de concretos con agregados reciclados |
title_sort |
Propiedades mecánicas, eléctricas y de durabilidad de concretos con agregados reciclados |
dc.creator.fl_str_mv |
Valverde Valverde, Jorge Alejandro Torres Castellanos, Nancy |
dc.contributor.author.spa.fl_str_mv |
Valverde Valverde, Jorge Alejandro Torres Castellanos, Nancy |
dc.subject.spa.fl_str_mv |
Agregados reciclados Resistencia a la comprensión Propiedades mecánicas Durabilidad |
topic |
Agregados reciclados Resistencia a la comprensión Propiedades mecánicas Durabilidad Comprensión - Pruebas Materiales - Propiedades mecánicas Comprehension - Testing Material - Mechanical properties Recycled aggregates Resistance to understanding Mechanical properties Durability |
dc.subject.armarc.spa.fl_str_mv |
Comprensión - Pruebas Materiales - Propiedades mecánicas |
dc.subject.armarc.eng.fl_str_mv |
Comprehension - Testing Material - Mechanical properties |
dc.subject.keywords.spa.fl_str_mv |
Recycled aggregates Resistance to understanding Mechanical properties Durability |
description |
The purpose of this article is to present the assessment of some of the electrical, mechanical and durability properties of concrete mixtures with replacement of coarse aggregate by aggregates of recycled concrete (ACR). The ACR used in the mixtures of the tests was produced from the crushing of concrete specimens, which had been tested in the laboratory of the Colombian School of Engineering. Eight mixtures with four contents of recycled aggregates (0%, 25%, 50% and 100%) and two values of water / cement ratio (0.5 and 0.6) were evaluated. Among the properties analyzed are the compression resistance, modulus of elasticity, resistivity, impedance, ultrasonic pulse velocity, permeability to the chloride ion, carbonation and thickeness. The results of the tests clearly indicated that in the mixtures with the highest percentage of recycled aggregate, the results of the modulus of elasticity and the resistance to compression are lower than for concretes with natural aggregate. The resistance to compression of a concrete with 100% ACR has an estimated reduction of 20 to 25%, with respect to a conventional concrete. At the same time, the electrical properties and the durability measured by resistivity, impedance, permeability and chloride ion permeability, and sorptivity tests are affected by the increase in the percentage of recycled aggregate and the water / cement ratio. |
publishDate |
2017 |
dc.date.issued.spa.fl_str_mv |
2017 |
dc.date.accessioned.spa.fl_str_mv |
2018-12-03T19:42:09Z |
dc.date.available.spa.fl_str_mv |
2018-12-03T19:42:09Z |
dc.date.accessioned.none.fl_str_mv |
2021-10-01T18:59:58Z |
dc.date.available.none.fl_str_mv |
2021-10-01T18:59:58Z |
dc.type.spa.fl_str_mv |
Artículo de revista |
dc.type.coar.fl_str_mv |
http://purl.org/coar/resource_type/c_2df8fbb1 |
dc.type.coarversion.fl_str_mv |
http://purl.org/coar/version/c_970fb48d4fbd8a85 |
dc.type.version.spa.fl_str_mv |
info:eu-repo/semantics/publishedVersion |
dc.type.coar.spa.fl_str_mv |
http://purl.org/coar/resource_type/c_6501 |
dc.type.content.spa.fl_str_mv |
Text |
dc.type.driver.spa.fl_str_mv |
info:eu-repo/semantics/article |
dc.type.redcol.spa.fl_str_mv |
http://purl.org/redcol/resource_type/ART |
format |
http://purl.org/coar/resource_type/c_6501 |
status_str |
publishedVersion |
dc.identifier.uri.spa.fl_str_mv |
http://revistas.escuelaing.edu.co/index.php/reci/article/view/15/11 |
dc.identifier.uri.none.fl_str_mv |
https://repositorio.escuelaing.edu.co/handle/001/885 |
url |
http://revistas.escuelaing.edu.co/index.php/reci/article/view/15/11 https://repositorio.escuelaing.edu.co/handle/001/885 |
dc.language.iso.spa.fl_str_mv |
spa |
language |
spa |
dc.relation.references.spa.fl_str_mv |
Al Khaleefi, A. & Almutairi, N. (2007). Ultrasonic pulse testing, chloride content and sulphate content of recycled concrete as coarse aggregate. Our World in Concrete & Structures. Singapur. Arriaga, L. E. (2013). Utilización de agregado grueso de concreto reciclado en elementos estructurales de concreto reforzado (tesis de maestría). Escuela Colombiana de Ingeniería Julio Garavito, Bogotá. Asociación Española de Gestores de Residuos de Construcción y Demolición (noviembre de 2010). Control de los residuos de construcción y demolición en los ayuntamientos. España. Asocreto (2011). Agregados reciclados presentes en la rehabilitación de estructuras. Asocreto, 108, 62. ASTM C1202-12 (s.f.). Standard Test Method for Electrical Indication of Concrete´s Ability to Resist Chloride Ion Penetration. ASTM C1585-11 (s.f.). Standard Test Method for Measurement of Rate of Absorption of Water by Hydraulic-Cement Concretes. Bojacá, N. R. (2013). Propiedades mecánicas y de durabilidad de concretos con agregados reciclados (tesis de maestría). Escuela Colombiana de Ingeniería Julio Garavito, Bogotá. Buozón Orgeira, N. (2011). Evaluación del proceso de hidratación de morteros de cemento con ceniza volante mediante métodos destructivos y no destructivos (tesis de maestría). Universidad Politécnica de Valencia, Valencia, España. Cassiano, J. (2010). Valoración de propiedades eléctricas del concreto y su correlación con algunas propiedades mecánicas y de durabilidad (tesis de maestría). Escuela Colombiana de Ingeniería Julio Garavito, Bogotá. Cement & Concrete Association from New Zeland (2011). Best practice guide for the use of recycled aggregates in new concrete. Nueva Zelanda. Coambiente S.A. (2009). Gestión Integral de escombros. Anteproyecto para la gestión integral de los RC&D en el Distrito Capital. Bogotá. Cortina Ramírez, J. M. (2007). Guía para el manejo de residuos sólidos generados en la industria de la construcción. Cholula, Puebla, México. Cruz. J.M., Landine, J., Lalinde, L.F. & Fita, I.C. (2010). Evaluación de las propiedades eléctricas de morteros de cemento con puzolanas(tesis de maestría). Universidad Politécnica de Valencia, Valencia España. Desai, S.B. & Limbachiya, M.C. (2006). Coarse recycled aggregate – a sustainable concrete solution. The Indian Concrete Journal, 17-23. ACC Limited Maharashtra. Exteberria, M., Vásquez, E. & Marí, A.R. (2007). Influence of amount or fecycled coarse aggregates and production process on properties of recycled aggregate concrete. Cement and Concrete Research, 735-742. Froudinston-Yannas, S. (1977). Waste concrete as aggregate fort new concrete. ACI Journal. Fuertes, A. (2012). Hacia un desarrollo sostenible en la producción de concreto a partir de desechos de construcción de mampostería de arcilla. Bogotá. Grace Construction Products (2006). Technical Bulletin TB - 0100 Understanding AASHTO T277 y ASTM C1202 Rapid Chloride Permeability Test. Guzmán, D. S. (2002). Durabilidad y patología del concreto. Bogotá: Instituto del Concreto, Asocreto. Kang, T.-K., Kim, W., Kwak, Y.-K., & Hong, S.-G. (2012). The choice of recycled concrete aggregate for flexural members. Proceedings of 18th International Association for Bridge and Structural Engineering Congress on Innovative Infraestructure. Seúl. Limbachiya et al. (2000). Use of recycled aggregate in highstrength concrete. Materials and Structures, 574-580. Lizarazo, J. (2008). Ensayos típicos en la determinación de la durabilidad del concreto. Seminario ACI. Ataque químico en el concreto. Maruyama, I. S. (2004). Flexural properties of reinforced recycled beams. Proceedings of International Rilem Conference on the Use of Recycled Materials in Buildings and Structures, 525-535. Maruyama, I., Sogo, M., Sobage, T., Sato, R. & Kawai, K. (2004). Flexural properties of reinforced recycled beams. Proceedings of International Rilem Conference on the Use of Recycled Materials in Bulidings and Structures. McNeil, K. & Thomas, H. & Kang, K. (2013). Recycled Concrete Aggregates: A Review. Estados Unidos. Natalani, M.B., Klees, D.R. & Tirner, J. (2000). Reciclaje y reutilizaciónde materiales residuales de construcción y demolición. Argentina: Universidad Nacional del Nordeste Argentina. Norma española UNE 83988-1 (2008). Durabilidad del hormigón. Método de ensayo. Determinación de la resistividad eléctrica, parte 1: Método directo (método de referencia). NSR-10 (s.f.). Reglamento Colombiano de Construcción Sismoresistente. Pinzón, H. (2009). Valoración de algunas propiedades del concreto adicionado con vidrio pulverizado. Bogotá. Corral Higuera, R., Arredondo-Rea, S.P., Neri Flores, M.A., Gómez- Soberón, J.M., Almaral Sánchez, J.L., Casterona González, J.H., Martínez Villafane, A., & Almeraya Calderón, F. (2011). Chloride Ion Penetrability and Corrosion Behavior of Steel in Concrete with Sustainability Characteristics. Rashwan, M.S. & Abourizh, S. (1997). The Properties of Recycled Concrete. Concrete. Estados Unidos. Rebolledo, N. R. (2010). Aplicación de técnicas no destructivas al estudio del hormigón fresco (tesis de maestría). Madrid: Universidad Politécnica de Madrid. Shayan, A. & Xu, A. (2003). Performance and properties of structural concrete made with recycled concrete aggregate. ACI Materials Journal 100(5), 371-380. Torres, N. (2009). Valoración del paso de cloruros en concretos con diferentes características. Boletín técnico de la seccional Colombiana del Instituto Americano del Concreto ACI. Bogotá: Universidad Nacional de Colombia. Torres, N. (2010). Concreto con agregados provenientes de escombros de construcción y demolición en Colombia. Boletín Técnico de la Seccional Colombiana del Instituto Americano del Concreto ACI. Yang, K., Chung, H.-S. & Ashour, A. (2008). Influence of Type and Replacement Level of Recycled Aggregates on Concrete Properties. ACI Materials Journal. Zhang, M. I. (2009). Recycled Concrete Aggregate and its Application in New Zealand Ready Mixed Production. New Zealand Concrete Industries Conference. |
dc.rights.spa.fl_str_mv |
Derechos Reservados - Escuela Colombiana de Ingeniería Julio Garavito |
dc.rights.coar.fl_str_mv |
http://purl.org/coar/access_right/c_abf2 |
dc.rights.uri.spa.fl_str_mv |
https://creativecommons.org/licenses/by-nc/4.0/ |
dc.rights.accessrights.spa.fl_str_mv |
info:eu-repo/semantics/openAccess |
dc.rights.creativecommons.spa.fl_str_mv |
Atribución-NoComercial 4.0 Internacional (CC BY-NC 4.0) |
rights_invalid_str_mv |
Derechos Reservados - Escuela Colombiana de Ingeniería Julio Garavito https://creativecommons.org/licenses/by-nc/4.0/ Atribución-NoComercial 4.0 Internacional (CC BY-NC 4.0) http://purl.org/coar/access_right/c_abf2 |
eu_rights_str_mv |
openAccess |
dc.format.mimetype.spa.fl_str_mv |
application/pdf |
dc.publisher.spa.fl_str_mv |
Escuela Colombiana de Ingeniería Julio Garavito |
dc.source.spa.fl_str_mv |
Revista de la Escuela Colombiana de Ingeniería; Núm. 108 (2017): Revista Nº 108 Octubre - Diciembre; p 15-23 0121-5132 |
institution |
Escuela Colombiana de Ingeniería Julio Garavito |
bitstream.url.fl_str_mv |
https://repositorio.escuelaing.edu.co/bitstream/001/885/1/Propiedades%20mec%c3%a1nicas%2c%20el%c3%a9ctricas%20y%20de%20durabilidad%20de%20concretos%20con%20agregados%20reciclados.pdf https://repositorio.escuelaing.edu.co/bitstream/001/885/2/license.txt https://repositorio.escuelaing.edu.co/bitstream/001/885/4/Propiedades%20mec%c3%a1nicas%2c%20el%c3%a9ctricas%20y%20de%20durabilidad%20de%20concretos%20con%20agregados%20reciclados.pdf.txt https://repositorio.escuelaing.edu.co/bitstream/001/885/5/Propiedades%20mec%c3%a1nicas%2c%20el%c3%a9ctricas%20y%20de%20durabilidad%20de%20concretos%20con%20agregados%20reciclados.pdf.jpg |
bitstream.checksum.fl_str_mv |
86f56725801508956806dad04d69c8f8 5a7ca94c2e5326ee169f979d71d0f06e 32b2d8f8ad466900fe733a1f54f64165 25f459e73df2c6a84cffef8d30cf4da8 |
bitstream.checksumAlgorithm.fl_str_mv |
MD5 MD5 MD5 MD5 |
repository.name.fl_str_mv |
Repositorio Escuela Colombiana de Ingeniería Julio Garavito |
repository.mail.fl_str_mv |
repositorio.eci@escuelaing.edu.co |
_version_ |
1814355611895201792 |
spelling |
Valverde Valverde, Jorge Alejandro7cac6ca804a72a0a684611f5ff98e0a1600Torres Castellanos, Nancy2b475ecd9ea004cd3b18c2eaf60c01d16002018-12-03T19:42:09Z2021-10-01T18:59:58Z2018-12-03T19:42:09Z2021-10-01T18:59:58Z2017http://revistas.escuelaing.edu.co/index.php/reci/article/view/15/11https://repositorio.escuelaing.edu.co/handle/001/885The purpose of this article is to present the assessment of some of the electrical, mechanical and durability properties of concrete mixtures with replacement of coarse aggregate by aggregates of recycled concrete (ACR). The ACR used in the mixtures of the tests was produced from the crushing of concrete specimens, which had been tested in the laboratory of the Colombian School of Engineering. Eight mixtures with four contents of recycled aggregates (0%, 25%, 50% and 100%) and two values of water / cement ratio (0.5 and 0.6) were evaluated. Among the properties analyzed are the compression resistance, modulus of elasticity, resistivity, impedance, ultrasonic pulse velocity, permeability to the chloride ion, carbonation and thickeness. The results of the tests clearly indicated that in the mixtures with the highest percentage of recycled aggregate, the results of the modulus of elasticity and the resistance to compression are lower than for concretes with natural aggregate. The resistance to compression of a concrete with 100% ACR has an estimated reduction of 20 to 25%, with respect to a conventional concrete. At the same time, the electrical properties and the durability measured by resistivity, impedance, permeability and chloride ion permeability, and sorptivity tests are affected by the increase in the percentage of recycled aggregate and the water / cement ratio.El propósito de este artículo es presentar la valoración de algunas de las propiedades eléctricas, mecánicas y de durabilidad de mezclas de concreto con remplazo de agregado grueso por agregados de concreto reciclado (ACR). El ACR usado en las mezclas de los ensayos se produjo a partir de la trituración de probetas de concreto, las cuales se habían ensayado en el laboratorio de la Escuela Colombiana de Ingeniería. Se evaluaron ocho mezclas con cuatro contenidos de agregados reciclado (0 %, 25 %, 50 % y 100 %) y dos valores de relación agua/cemento (0,5 y 0,6). Entre las propiedades analizadas están la resistencia a la compresión, módulo de elasticidad, resistividad, impedancia, velocidad de pulso ultrasónico, permeabilidad al ion cloruro, carbonatación y sortividad. Los resultados de los ensayos indicaron claramente que en las mezclas con mayor porcentaje de agregado reciclado, los resultados del módulo de elasticidad y la resistencia a la compresión son más bajos que para concretos con agregado natural. La resistencia a la compresión de un concreto con 100 % de ACR tiene una reducción estimada del 20 al 25 %, con respecto a un concreto convencional. Paralelamente, las propiedades eléctricas y la durabilidad medida mediante ensayos de resistividad, impedancia, sortividad y permeabilidad al ion cloruro, y sortividad, se ven afectadas con el aumento del porcentaje de agregado reciclado y la relación agua/cemento.application/pdfspaEscuela Colombiana de Ingeniería Julio GaravitoDerechos Reservados - Escuela Colombiana de Ingeniería Julio Garavitohttps://creativecommons.org/licenses/by-nc/4.0/info:eu-repo/semantics/openAccessAtribución-NoComercial 4.0 Internacional (CC BY-NC 4.0)http://purl.org/coar/access_right/c_abf2Revista de la Escuela Colombiana de Ingeniería; Núm. 108 (2017): Revista Nº 108 Octubre - Diciembre; p 15-230121-5132Agregados recicladosResistencia a la comprensiónPropiedades mecánicasDurabilidadComprensión - PruebasMateriales - Propiedades mecánicasComprehension - TestingMaterial - Mechanical propertiesRecycled aggregatesResistance to understandingMechanical propertiesDurabilityPropiedades mecánicas, eléctricas y de durabilidad de concretos con agregados recicladosArtículo de revistainfo:eu-repo/semantics/publishedVersionhttp://purl.org/coar/resource_type/c_6501http://purl.org/coar/resource_type/c_2df8fbb1Textinfo:eu-repo/semantics/articlehttp://purl.org/redcol/resource_type/ARThttp://purl.org/coar/version/c_970fb48d4fbd8a85Al Khaleefi, A. & Almutairi, N. (2007). Ultrasonic pulse testing, chloride content and sulphate content of recycled concrete as coarse aggregate. Our World in Concrete & Structures. Singapur.Arriaga, L. E. (2013). Utilización de agregado grueso de concreto reciclado en elementos estructurales de concreto reforzado (tesis de maestría). Escuela Colombiana de Ingeniería Julio Garavito, Bogotá.Asociación Española de Gestores de Residuos de Construcción y Demolición (noviembre de 2010). Control de los residuos de construcción y demolición en los ayuntamientos. España.Asocreto (2011). Agregados reciclados presentes en la rehabilitación de estructuras. Asocreto, 108, 62.ASTM C1202-12 (s.f.). Standard Test Method for Electrical Indication of Concrete´s Ability to Resist Chloride Ion Penetration. ASTM C1585-11 (s.f.). Standard Test Method for Measurement of Rate of Absorption of Water by Hydraulic-Cement Concretes.Bojacá, N. R. (2013). Propiedades mecánicas y de durabilidad de concretos con agregados reciclados (tesis de maestría). Escuela Colombiana de Ingeniería Julio Garavito, Bogotá.Buozón Orgeira, N. (2011). Evaluación del proceso de hidratación de morteros de cemento con ceniza volante mediante métodos destructivos y no destructivos (tesis de maestría). Universidad Politécnica de Valencia, Valencia, España.Cassiano, J. (2010). Valoración de propiedades eléctricas del concreto y su correlación con algunas propiedades mecánicas y de durabilidad (tesis de maestría). Escuela Colombiana de Ingeniería Julio Garavito, Bogotá.Cement & Concrete Association from New Zeland (2011). Best practice guide for the use of recycled aggregates in new concrete. Nueva Zelanda.Coambiente S.A. (2009). Gestión Integral de escombros. Anteproyecto para la gestión integral de los RC&D en el Distrito Capital. Bogotá.Cortina Ramírez, J. M. (2007). Guía para el manejo de residuos sólidos generados en la industria de la construcción. Cholula, Puebla, México.Cruz. J.M., Landine, J., Lalinde, L.F. & Fita, I.C. (2010). Evaluación de las propiedades eléctricas de morteros de cemento con puzolanas(tesis de maestría). Universidad Politécnica de Valencia, Valencia España.Desai, S.B. & Limbachiya, M.C. (2006). Coarse recycled aggregate – a sustainable concrete solution. The Indian Concrete Journal, 17-23. ACC Limited Maharashtra.Exteberria, M., Vásquez, E. & Marí, A.R. (2007). Influence of amount or fecycled coarse aggregates and production process on properties of recycled aggregate concrete. Cement and Concrete Research, 735-742.Froudinston-Yannas, S. (1977). Waste concrete as aggregate fort new concrete. ACI Journal.Fuertes, A. (2012). Hacia un desarrollo sostenible en la producción de concreto a partir de desechos de construcción de mampostería de arcilla. Bogotá.Grace Construction Products (2006). Technical Bulletin TB - 0100 Understanding AASHTO T277 y ASTM C1202 Rapid Chloride Permeability Test.Guzmán, D. S. (2002). Durabilidad y patología del concreto. Bogotá: Instituto del Concreto, Asocreto.Kang, T.-K., Kim, W., Kwak, Y.-K., & Hong, S.-G. (2012). The choice of recycled concrete aggregate for flexural members.Proceedings of 18th International Association for Bridge and Structural Engineering Congress on Innovative Infraestructure. Seúl.Limbachiya et al. (2000). Use of recycled aggregate in highstrength concrete. Materials and Structures, 574-580.Lizarazo, J. (2008). Ensayos típicos en la determinación de la durabilidad del concreto. Seminario ACI. Ataque químico en el concreto.Maruyama, I. S. (2004). Flexural properties of reinforced recycled beams. Proceedings of International Rilem Conference on the Use of Recycled Materials in Buildings and Structures, 525-535.Maruyama, I., Sogo, M., Sobage, T., Sato, R. & Kawai, K. (2004). Flexural properties of reinforced recycled beams. Proceedings of International Rilem Conference on the Use of Recycled Materials in Bulidings and Structures.McNeil, K. & Thomas, H. & Kang, K. (2013). Recycled Concrete Aggregates: A Review. Estados Unidos.Natalani, M.B., Klees, D.R. & Tirner, J. (2000). Reciclaje y reutilizaciónde materiales residuales de construcción y demolición. Argentina: Universidad Nacional del Nordeste Argentina.Norma española UNE 83988-1 (2008). Durabilidad del hormigón. Método de ensayo. Determinación de la resistividad eléctrica, parte 1: Método directo (método de referencia).NSR-10 (s.f.). Reglamento Colombiano de Construcción Sismoresistente.Pinzón, H. (2009). Valoración de algunas propiedades del concreto adicionado con vidrio pulverizado. Bogotá.Corral Higuera, R., Arredondo-Rea, S.P., Neri Flores, M.A., Gómez- Soberón, J.M., Almaral Sánchez, J.L., Casterona González, J.H., Martínez Villafane, A., & Almeraya Calderón, F. (2011). Chloride Ion Penetrability and Corrosion Behavior of Steel in Concrete with Sustainability Characteristics.Rashwan, M.S. & Abourizh, S. (1997). The Properties of Recycled Concrete. Concrete. Estados Unidos.Rebolledo, N. R. (2010). Aplicación de técnicas no destructivas al estudio del hormigón fresco (tesis de maestría). Madrid: Universidad Politécnica de Madrid.Shayan, A. & Xu, A. (2003). Performance and properties of structural concrete made with recycled concrete aggregate. ACI Materials Journal 100(5), 371-380.Torres, N. (2009). Valoración del paso de cloruros en concretos con diferentes características. Boletín técnico de la seccional Colombiana del Instituto Americano del Concreto ACI. Bogotá: Universidad Nacional de Colombia.Torres, N. (2010). Concreto con agregados provenientes de escombros de construcción y demolición en Colombia. Boletín Técnico de la Seccional Colombiana del Instituto Americano del Concreto ACI.Yang, K., Chung, H.-S. & Ashour, A. (2008). Influence of Type and Replacement Level of Recycled Aggregates on Concrete Properties. ACI Materials Journal.Zhang, M. I. (2009). Recycled Concrete Aggregate and its Application in New Zealand Ready Mixed Production. New Zealand Concrete Industries Conference.ORIGINALPropiedades mecánicas, eléctricas y de durabilidad de concretos con agregados reciclados.pdfapplication/pdf1232739https://repositorio.escuelaing.edu.co/bitstream/001/885/1/Propiedades%20mec%c3%a1nicas%2c%20el%c3%a9ctricas%20y%20de%20durabilidad%20de%20concretos%20con%20agregados%20reciclados.pdf86f56725801508956806dad04d69c8f8MD51open accessLICENSElicense.txttext/plain1881https://repositorio.escuelaing.edu.co/bitstream/001/885/2/license.txt5a7ca94c2e5326ee169f979d71d0f06eMD52open accessTEXTPropiedades mecánicas, eléctricas y de durabilidad de concretos con agregados reciclados.pdf.txtPropiedades mecánicas, eléctricas y de durabilidad de concretos con agregados reciclados.pdf.txtExtracted texttext/plain42995https://repositorio.escuelaing.edu.co/bitstream/001/885/4/Propiedades%20mec%c3%a1nicas%2c%20el%c3%a9ctricas%20y%20de%20durabilidad%20de%20concretos%20con%20agregados%20reciclados.pdf.txt32b2d8f8ad466900fe733a1f54f64165MD54open accessTHUMBNAILPropiedades mecánicas, eléctricas y de durabilidad de concretos con agregados reciclados.pdf.jpgPropiedades mecánicas, eléctricas y de durabilidad de concretos con agregados reciclados.pdf.jpgGenerated Thumbnailimage/jpeg14162https://repositorio.escuelaing.edu.co/bitstream/001/885/5/Propiedades%20mec%c3%a1nicas%2c%20el%c3%a9ctricas%20y%20de%20durabilidad%20de%20concretos%20con%20agregados%20reciclados.pdf.jpg25f459e73df2c6a84cffef8d30cf4da8MD55open access001/885oai:repositorio.escuelaing.edu.co:001/8852022-08-10 10:43:07.954open accessRepositorio Escuela Colombiana de Ingeniería Julio Garavitorepositorio.eci@escuelaing.edu.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 |